Tanperati chanm gerikolan793 se ajan geri ki konpoze de de konpozan, ak endikatè teknik li yo yo montre nan tablo ki anba la a.
Lèt | 793 |
aparisyon | Transparan, inifòm ak gratis nan enpurte |
Kontni solid (120 ℃ ± 5 ℃, 2H) | 50%-60% |
Rezistivite sifas yo | ≥1 × 1012Ω |
1. Aparans: Evalyasyon pa obsèvasyon vizyèl.
2. Solid content: After mixing the two components of Room temperature curing epoxy dipping adhesive 793 according to the required ratio and stirring evenly, add 1.5~2g glue to the vessel to make it evenly distributed on the bottom of the vessel, after placing it in the air for 30min, place it horizontally at 120℃±5℃ In the oven, bake for 2h, after the sample is taken out, it se refwadi a tanperati chanm nan yon desikateur, ak Lè sa a, te peze pou kalkil.
3. Surface resistivity: After mixing the two components of 793 according to the required ratio and stirring evenly, paint a layer on the 100×100 insulating board (thickness ≤ 2mm), dry it at room temperature for 20 minutes, and then put it in an oven at 120 ℃ Bake at ±5℃ for 2h, cool to room temperature naturally, and measure with a high resistancemèt.
1. Tanperati chanm geri epoksidik tranpe adezif 793 se pake nan de konpozan, ak yon pwa minimòm de 5kg pou chak barik pwa maksimòm pou chak barik se 20kg.
2. Peryòd nan depo nan eleman sèl nan tanperati chanm nan se 12 mwa soti nan dat la nan fabrike.
3. Si pwodwi a depase peryòd la depo ak pase enspeksyon an, li kapab itilize ankò.
Melanje tanperati chanm nan geri epoksidik tranpe adezif 793 konpozan ansanm selon pwopòsyon an, epi imedyatman brase kontinyèlman pou plis pase 5 minit. Apre brase respire, li kapab itilize. Tanperati a prepare chanm geri epoksidik adezif yo dwe itilize moute nan 8 èdtan.